Hey guys, I'd like to get your opinion on a couple things. I will start off saying I've read the TECH FAQ about reinforcing numerous times, but I would still like to get the opinions from those who have done this a couple times and have some experience.
I plan on doing my engine bay, nose, pole bracket, then installing some Matt Smith Style holds. After riding with him, I love them and the flexibility of riding positions. http://www.x-h2o.com/threads/97521-MattSmith-America-Ski-SJ-Build
My questions really go out to how much material do I need? I ride the soft about 20 percent and flat 80 percent. This summer has been nothing but surf 3+ days a week because I've been lucky enough to be located and working close to Oceanside, Ca. My Flatwater only ski is starting to take a beating and showing signs of it.
I plan on using 17oz biax, 2 layers and top it with 5.7 oz 2x2 twill for a little bling effect. Do you think this is a good choice? I see some using 12oz?
5 yards of 17 oz?
2 yards of 2x2 CF twill?
2 Gallons of resign 2:1 which will equate to 3 overall gallons. Being told I need this much, better to be safe then sorry? It's hot, need slow cure too.
Some pumps and misc materials.
Pour Foam... How much? What Density? Will be moving the exhaust tube down.
Then Just a quart of Microballons to fill bond lines? More?
a roller
SHARP SCISSORS
Im working with someone who has laid carbon in the past and IMO has done great job. By no means an EXPERT but far better than the average JOE who has never done it before. I understand it is fragile and harder to work with.
Please chime in with anything, materials and quantity of materials needed, opinions... anything...
THANKS!
I plan on doing my engine bay, nose, pole bracket, then installing some Matt Smith Style holds. After riding with him, I love them and the flexibility of riding positions. http://www.x-h2o.com/threads/97521-MattSmith-America-Ski-SJ-Build
My questions really go out to how much material do I need? I ride the soft about 20 percent and flat 80 percent. This summer has been nothing but surf 3+ days a week because I've been lucky enough to be located and working close to Oceanside, Ca. My Flatwater only ski is starting to take a beating and showing signs of it.
I plan on using 17oz biax, 2 layers and top it with 5.7 oz 2x2 twill for a little bling effect. Do you think this is a good choice? I see some using 12oz?
5 yards of 17 oz?
2 yards of 2x2 CF twill?
2 Gallons of resign 2:1 which will equate to 3 overall gallons. Being told I need this much, better to be safe then sorry? It's hot, need slow cure too.
Some pumps and misc materials.
Pour Foam... How much? What Density? Will be moving the exhaust tube down.
Then Just a quart of Microballons to fill bond lines? More?
a roller
SHARP SCISSORS
Im working with someone who has laid carbon in the past and IMO has done great job. By no means an EXPERT but far better than the average JOE who has never done it before. I understand it is fragile and harder to work with.
Please chime in with anything, materials and quantity of materials needed, opinions... anything...