Custom/Hybrid Vinylester resin

I bought some Vinylester resin today, the came with no instructions on how to mix it. I bought it from a local shop that has new owners and they don't know anything about composite materials. It came with 2 hardeners (Cobalt and DMA) and I have no idea what the mix ratio is
 

tomski

X
Location
LHC
Cobalt is a promoter for heat curing. Dma is for an accelerator for faster curing.

Use mekp for room temperature curing at 2%.
 
Cobalt is a promoter for heat curing. Dma is for an accelerator for faster curing.

Use mekp for room temperature curing at 2%.
Thanks, I've talked to a few different people now and the consensus seems to be 0.1% DMA and 0.1% Cobalt, then mix in 1-2% MEKP.

Is it true that if MEKP and DMA are mixed it will cause an explosion?
 

227

Its all about the surf!
Location
Oceanside, CA
Whats the difference between Vinylester and Polyester? Everything I've used except West systems 2 part epoxy turned out to be a mistake.
 

tomski

X
Location
LHC
Thanks, I've talked to a few different people now and the consensus seems to be 0.1% DMA and 0.1% Cobalt, then mix in 1-2% MEKP.

Is it true that if MEKP and DMA are mixed it will cause an explosion?

That's a good question. I use vinylester and only mekp in room temperature curing. But I use different catalysts for temperatures here in the desert.
 
Last edited:

tomski

X
Location
LHC
I would do a test batch before any major work. I've never used DMA and Cobalt; different processes would use them. Right now I use Composites One Vinylester Resin.
 
Top Bottom