I am going to reinforce my roundnose, and add some footholds to it as well. The nose was already done by the previous owner, so I will not have to mess with that. I will be doing the sides and the hoodseal area. To fill the bondline I plan on using epoxy resin mixed with cabosil or chopped strand fiberglass(which one????) Then I plan on using a single layer of 17oz biaxial for the sides. I was debating on whether to use 1 or 2 layers, then I read in a thread that Taylor Curtis only uses one layer of 17oz with a layer of CF on top of that. I'm only a flat water rider that hasn't pulled any rolls yet, but I will learn this season, so I think one layer should be ok for me. Let me know what you guys think about the 1 layer. I want to keep this boat light, and I don't want any pipe clearance issues. For the hoodseal area, should I just cut a couple of strips of biaxial or should I use epoxy and chopped strand for that? I need some tips here.
My List of stuff:
17oz biaxial- have to measure yet.
1 gallon on thin epoxy resin quick drying. I'm a fiberglass rookie, should I get quick or medium?
4lb tub of 1/2 chopped strand
1 qt of Cabosil
a couple of squegies.
Take a look at this and please let me know if I'm missing anything. I realize that there are other threads about this, but none of them answered my specific questions. Thanks in advance guys.
Also for the footholds, should I just cut up some strips of 17oz to glass those in?
My List of stuff:
17oz biaxial- have to measure yet.
1 gallon on thin epoxy resin quick drying. I'm a fiberglass rookie, should I get quick or medium?
4lb tub of 1/2 chopped strand
1 qt of Cabosil
a couple of squegies.
Take a look at this and please let me know if I'm missing anything. I realize that there are other threads about this, but none of them answered my specific questions. Thanks in advance guys.
Also for the footholds, should I just cut up some strips of 17oz to glass those in?