Little up date. I went and picked up some parts from Blowsion. I got this and my cold fusion internal fuel fill, worx intake grate and new hood seal. I got most the pull bracket area and fuel fill area sanded.
Question, would puting two layers of 1208 over the old fuel filler hole be enough or...
Newb question that I could quite find the answer two. She. Doing two layers of 1208 bixial glass do I need to let the first layer dry first then sand or can I get the first layer on and wet and add the second?
Sent from my XT1030 using Tapatalk
So do I need to use twill? Also do I add cabosal to the epoxy when laying the fiber glass or is that just for filling areas?
Sent from my XT1030 using Tapatalk
Okay, would it be more beneficial to use Kevlar or carbon fiber? Carbon fiber is probably not sandable for a good out side finish?